Căutare după Subiect "nitriding"
Afișează articolele 1-6 of 6
-
Behavior of Rp3-High Spped on Short Time Nitriding in Fluidized Bed
(Universitatea "Dunărea de Jos" din Galați, 2005)For steel nitriding, treatment time is a important factor. Gas and plasma nitriding are usual method to increase surface properties by nitriding. A close retort is used. Total time for treatment are higher because are ... -
Behaviour at Nitriding in Fluidized Layer of Austenitic Stainless Steels at the Temperature
(Universitatea "Dunărea de Jos" din Galați, 2007)Nitriding at low temperatures, 450-500oC of austenic stainless steels lead to the obtaining of the tough layers over 1000 HV005 but having thicknesses of tenths of microns. Moreover, nitriding at 500ºC has determined the ... -
Behaviour at Nitriding in Fluidized Layer of Austenitic Stainless Steels at the Temperature of 450°C
(Universitatea "Dunărea de Jos" din Galați, 2007)Stainless austenitic steels have a good corrosion resistance but reduced abrasion strength due to low strength below 200HV5. By nitriding one may ensure the obtaining of a superficial layer with increased strength that ... -
Nanostructured Surface for 38MoCrA109 Steel by Nitriding in Nitrogen Atmosphere and Yag;Nd Pulse Laser Activation
(Universitatea "Dunărea de Jos" din Galați, 2008)YAG:Nd pulse laser is usually used for cutting and welding. The paper is based by experiments using YAG:Nd pulse laser (KVANT 17-CIS made). Technological modules were assembled for laser beam deviation and for relative ... -
Surface Hardening of 40Cr10 steel After Short Time Nitriding in Fluidized Bed
(Universitatea "Dunărea de Jos" din Galați, 2006)The paper is based by nitriding in fluidized bed experiments over laboratory plant. Fluidization applications are characterized by high values of mass and heat transfer coefficients. For experiments were used 40Cr10 ... -
Surface Hardenining for 38MoCrA109 Steel Using Fluidized Bed Nitriding
(Universitatea "Dunărea de Jos" din Galaţi, 2008)The paper is based an nitriding experiments made in a fluidized bed laboratory furnace. Fluidization was obtained in a steel refractory retort by solid granular (burned fire clay) and fluid (mixture of ammonia and ...