Arată înregistrarea sumară a articolului

dc.contributor.authorGrechanyuk, I. N.
dc.contributor.authorGrechanyuk, V. G.
dc.contributor.authorArtuh, Y. U.
dc.date.accessioned2018-11-07T07:51:20Z
dc.date.available2018-11-07T07:51:20Z
dc.date.issued2009
dc.identifier.issn1453 – 083X
dc.identifier.urihttp://10.11.10.50/xmlui/handle/123456789/5637
dc.descriptionTHE ANNALS OF “DUNAREA DE JOS” UNIVERSITY OF GALATI. FASCICLE IX. METALLURGY AND MATERIALS SCIENCE N0. 1 – 2009, ISSN 1453 – 083Xro_RO
dc.description.abstractThe article is devoted to the study of corrosive and thermal stability of materials composition on the basis of copper, obtained by the EB-PVD method. It is shown in this work that corrosion of (Cu-Sn)–Mo composites have got the electrochemical mechanism from dissolution of a more active metal of molybdenum. Chemical composition of composite material affects corrosive properties of material: at the increase of maintenance of molybdenum in the copper matrix corrosive and thermal stability is decreasing, in comparison with the pure copper. The special decreasing of the corrosive stability is definite during concentration of molybdenum of about 12.56 %. This is explained by the considerable increase of quantity of micro-galvanic pairs.ro_RO
dc.language.isoenro_RO
dc.publisherUniversitatea "Dunărea de Jos" din Galațiro_RO
dc.subjectComposite Materialsro_RO
dc.subjectCorrosive and Thermal Stabilityro_RO
dc.titlePhysical-Chemical Properties (Cu-Sn) -Mo Composite Materialsro_RO